So folks, now i have update. I put these three buttons on XRF spectrometer, and results are 75 % - 82 % gold. Other metal its some kind of steel (Fe,Cr...). Method, that i am using is jaw vice, pliers, screwdriver and hammer. Now calculating, if theoretically every button has 75% gold and weight 0.03g, this is 0.0225g pure gold. I have cca 800pcs of theese diodes, next load wait
. If i am calculating correct, 18g (or more) of gold waiting for me :lol: .
If is somebody interrest, look for this types - 1NZ70, 2NZ70, 3NZ70, 4NZ70, 5NZ70, 6NZ70, 7NZ70, 8NZ70, 32NP75, 33NP75, 34NP75, 35NP75, 36NP75, 37NP75, 42NP75, 43NP75, 44NP75, 45NP75, 46NP75.
This forum give me a lot of information, so i have a need to give something to him. Sorry for my English
, i hope, you understand everything.
Thanks, have a nice day and nice buttons
.