Dear friends:
Thank you again for your help guys and sharing your knowledge.............
I want to ask about the stannous chloride test solution, when i add the SnCl2 to my AR ,my solution turn to transparent :roll: ?!! what does that mean ? too much nitric :?: ? i have no gold in my AR ? :shock:
Bearing in mind my stannous was made of SnCl2 "powder" dissolve in HCL , also my AR was made from dissolved CPU pin.
Any ideas ...........? :idea:
Best regards
Thank you again for your help guys and sharing your knowledge.............
I want to ask about the stannous chloride test solution, when i add the SnCl2 to my AR ,my solution turn to transparent :roll: ?!! what does that mean ? too much nitric :?: ? i have no gold in my AR ? :shock:
Bearing in mind my stannous was made of SnCl2 "powder" dissolve in HCL , also my AR was made from dissolved CPU pin.
Any ideas ...........? :idea:
Best regards