Noxx
Well-known member
Hello
Here is one lot I did last winter.
I started with 20grams of scrap gold
[img:640:480]http://goldrefiningforum.com/images/Gold%20Refining%20002.jpg[/img]
I processed everything outside on cold temp. (-20celcius) Thats why there is an hotplate.
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20010.jpg[/img]
I ended up with brown powder (actually gold !)
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20011.jpg[/img]
Closer look when dry
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20013.jpg[/img]
When I melted all the powder, voila, beautiful 24k gold nuggets.
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20016.jpg[/img]
There'll be more of my gold batches in the near future.
Here is one lot I did last winter.
I started with 20grams of scrap gold
[img:640:480]http://goldrefiningforum.com/images/Gold%20Refining%20002.jpg[/img]
I processed everything outside on cold temp. (-20celcius) Thats why there is an hotplate.
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20010.jpg[/img]
I ended up with brown powder (actually gold !)
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20011.jpg[/img]
Closer look when dry
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20013.jpg[/img]
When I melted all the powder, voila, beautiful 24k gold nuggets.
[img:640:480]http://goldrefiningforum.com/img/Gold%20Refining%20016.jpg[/img]
There'll be more of my gold batches in the near future.