Geo
Well-known member
well, here is what was in the AP bucket that i hurt myself over.it was not worth it but for some reason i felt i needed to at least show the fruits of what came from the situation.
20g of refined gold from one AP bucket isnt bad. ill try and list what i had in it
2+ pounds of cut fingers
3+ pounds of milspec pins
1 pound header pins
4 pounds of milspec boards with gold traces
4 pounds IC chips (processed in AR, not AP)
20g of refined gold from one AP bucket isnt bad. ill try and list what i had in it
2+ pounds of cut fingers
3+ pounds of milspec pins
1 pound header pins
4 pounds of milspec boards with gold traces
4 pounds IC chips (processed in AR, not AP)