Hi Guys, I am new here this place looks like a great place to share ideas and gain knowledge.
Anyhow I have a issue and would like to know if anyone could help.

I have leached my heavy gold cons using Sodium Thiosulfate and water mix. I had left them in the glass container for approximately 2 weeks stiring every so often and adding more crystals
Every few day to make sure the leach was strong. After the 2 weeks I filtered the solution using a coffee filter and i could see the colour had a slight yellow orange hue so I am assuming the gold an sliver salts had leached into solution? Now I have been trying to find a way to cement the gold out of the mix as it is not hydo or nitrc acid as water was used with the Thiosulfate. I am trying to stay away from acids if possible?. I was thinking electrowinning the solution with to stainless steel sheets. One as the anode an 1 as cathode would this work? I have attached a pic of solution does this look like gold particles floating around? I also put a piece or aluminum in the solution as it though it might drop the gold haha.

Any help would be awesome on trying to recover the metals 🤙
 

Attachments

  • 20241024_115009.jpg
    20241024_115009.jpg
    1.2 MB
  • 20241019_172414.jpg
    20241019_172414.jpg
    2.4 MB
Hi Guys, I am new here this place looks like a great place to share ideas and gain knowledge.
Anyhow I have a issue and would like to know if anyone could help.

I have leached my heavy gold cons using Sodium Thiosulfate and water mix. I had left them in the glass container for approximately 2 weeks stiring every so often and adding more crystals
Every few day to make sure the leach was strong. After the 2 weeks I filtered the solution using a coffee filter and i could see the colour had a slight yellow orange hue so I am assuming the gold an sliver salts had leached into solution? Now I have been trying to find a way to cement the gold out of the mix as it is not hydo or nitrc acid as water was used with the Thiosulfate. I am trying to stay away from acids if possible?. I was thinking electrowinning the solution with to stainless steel sheets. One as the anode an 1 as cathode would this work? I have attached a pic of solution does this look like gold particles floating around? I also put a piece or aluminum in the solution as it though it might drop the gold haha.

Any help would be awesome on trying to recover the metals 🤙
Welcome to us.
What kind of research did you do before you decided to go for Thio Sulfate?
It is one of the things that haunt us from time to time.
It puts Gold into solution all right, but it do not want to let it go.
Are you sure the Thio/water way is the way to go?
Do you even know if it works?
I did one little search and it seems it is slightly more involved than Thio/water, here is a link to one article.
https://www.sciencedirect.com/science/article/abs/pii/S0892687500001722

Anyway since you are already using chemicals I want you to study these links:
We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/


Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 
Hi Yggdrasil,
Thank you for your reply.
I have done a little bit of research on using sodium Thiosulfate as the leaching solution. I wanted to go down the greener way rather than using acids ect. I do also have copper sulfate crystals but I was going to try without using those first as it would be one less thing I would have to deal with. I am not fussed about the leach rate as time is not a factor. As I understand copper sulfate is used to speed up the leaching rate. I think I will try electrowinning the solution onto stainless sheets. I was going to try pour Zinc powder into the solution to drop the gold but not sure if that only works in acid not a water concentrate? Also I am having issues trying to purchase zinc powder as it is classed as a dangerous goods and I am not approved handler and not registered.

Thanks
Aaron

 
Hi Yggdrasil,
Thank you for your reply.
I have done a little bit of research on using sodium Thiosulfate as the leaching solution. I wanted to go down the greener way rather than using acids ect. I do also have copper sulfate crystals but I was going to try without using those first as it would be one less thing I would have to deal with. I am not fussed about the leach rate as time is not a factor. As I understand copper sulfate is used to speed up the leaching rate. I think I will try electrowinning the solution onto stainless sheets. I was going to try pour Zinc powder into the solution to drop the gold but not sure if that only works in acid not a water concentrate? Also I am having issues trying to purchase zinc powder as it is classed as a dangerous goods and I am not approved handler and not registered.

Thanks
Aaron

If you are going to use Zinc it has to be either acidic or caustic.
There will be no energy to drive the ion exchange unless it has a pH that is sufficiently off center (7).
Did you read the paper I sent a link to? They used Ammonia if I'm not mistaken.
We have many threads on the forum regarding Thio Sulfate leaching and I think that most if not all are in the "help me" category.
Which means they are failed and most are not resolved.
Regarding "green" the moment a leach has dissolved metal ions it no longer are "green" and will be considered toxic to life.
 
Ok thanks, I guess that's what the copper nitrate was used in studys for as it would cause the solution to turn more acidic and then the zinc would drop the gold I am guessing? The copper nitrate also degrades the Thiosulfate more rapidly. That's what the Ammonia is ment to combat. Bugger I not wanting to use Ammonia. I might try add some copper sulfate if this doesn't cement to the stainless. I am aware that any solutions containing waste/metals are toxic and will be delt with proper procedure.
 
Ok thanks, I guess that's what the copper nitrate was used in studys for as it would cause the solution to turn more acidic and then the zinc would drop the gold I am guessing? The copper nitrate also degrades the Thiosulfate more rapidly. That's what the Ammonia is ment to combat. Bugger I not wanting to use Ammonia. I might try add some copper sulfate if this doesn't cement to the stainless. I am aware that any solutions containing waste/metals are toxic and will be delt with proper procedure.
Why not go for something that actually work?
As I said, we have had this discussion multiple times in the past and I can't remember it going well any of those times.
 
Ok thanks, I guess that's what the copper nitrate was used in studys for as it would cause the solution to turn more acidic and then the zinc would drop the gold I am guessing? The copper nitrate also degrades the Thiosulfate more rapidly. That's what the Ammonia is ment to combat. Bugger I not wanting to use Ammonia. I might try add some copper sulfate if this doesn't cement to the stainless. I am aware that any solutions containing waste/metals are toxic and will be delt with proper procedure.
Have you found any reference what so ever that any of the major companies using this?
That is what we consider a litmus test in this community, if the major companies use it, it works.
If not, there are some snags to it.
Price, dealing with waste and practical use primarily.
 
The main reason the company's don't use it is the rate of Thiosulfate consumption i think I read somewhere it was 24kgs to the ton of ore so it is not really viable for the big companies at this stage. There is alot of research being put into this as it could potentially faze out cyanide use as a cleaner method. There is a issue with recovery on the activated charcoal for the big companys. But for the small scale miner it could work better price wise as I am only dealing with the heavy cons so there are not tons or ore to deal with. The big problem as you have been saying is finding a recovery method that works and not overly complicated
 
The main reason the company's don't use it is the rate of Thiosulfate consumption i think I read somewhere it was 24kgs to the ton of ore so it is not really viable for the big companies at this stage. There is alot of research being put into this as it could potentially faze out cyanide use as a cleaner method. There is a issue with recovery on the activated charcoal for the big companys. But for the small scale miner it could work better price wise as I am only dealing with the heavy cons so there are not tons or ore to deal with. The big problem as you have been saying is finding a recovery method that works and not overly complicated
If the concentrates are good it may be more sensible to smelt them.
 
I heard that You can precipitate the gold using
Ferrous sulfate.
or
Zinc.
or
FAS

i never use FAS before ,i have no experience with it.
I just heard about it
and of course I will not post the chemical name .

the precipitation
Is all depend in how You prepared the leaching solution

many peoples that are using Thiosulfate won’t reveal how they do it.

there is a company in Arizona that use Thiosulfate and with very good result.

but they spend lot of time and money
in how make their leach work.
so they won’t tell any one.

and of course the use of Ammonia
that is dangerous if You inhaled
 
Last edited:
I heard that You can precipitate the gold using
Ferrous sulfate.
Zinc.
Ammonium
Hi mate, I did a quick little test as I don't have much time atm. It looks like it can be electrowinning out onto stainless that was just about 5mins with a little 9v battery. You can clearly see the yellowish colour starting to form. This is awesome news 🍻
 

Attachments

  • 20241025_130838.jpg
    20241025_130838.jpg
    1.6 MB
Hi mate, I did a quick little test as I don't have much time atm. It looks like it can be electrowinning out onto stainless that was just about 5mins with a little 9v battery. You can clearly see the yellowish colour starting to form. This is awesome news 🍻
Good news I hope, not so good for your health I assume.
Get some gloves on your hands when you are working with chemicals mate.
There is one other reason Thio Sulfate is not much used, and that is that there are some indications it may be a carcinogen.
No Gold is worth your health.
 
You should be able to cement the gold out of solution using a piece of copper and ion exchange. I have done this with thiosulphate and it worked. Just add some generic cleaning ammonia to raise the ph to around 10 hang a copper sheet in the solution, stir or aerate. Or electrowinn.
 
You should be able to cement the gold out of solution using a piece of copper and ion exchange. I have done this with thiosulphate and it worked. Just add some generic cleaning ammonia to raise the ph to around 10 hang a copper sheet in the solution, stir or aerate. Or electrowinn.
Awesome will have to give that one a try.
Do those particles at the bottom an floating around suspended in the solution not look like gold already cemented? Could i not just strain the solution to get the particles then elecrtowinn the strained solution to get the rest that didn't cement out onto a peice of stainless? or is that alot of extra work as the liquid is still quite yellow so I guess there's still more in solution?

Thanks
Aaron
 
You should be able to cement the gold out of solution using a piece of copper and ion exchange. I have done this with thiosulphate and it worked. Just add some generic cleaning ammonia to raise the ph to around 10 hang a copper sheet in the solution, stir or aerate. Or electrowinn.
How would I also know the Ph level is there some test I can perform?
 
These test papers are excellent and the color scale is on each strip. If you need to be more precise they are available in short ranges for more precise determinations.

The advantage of the color scale on the test strip is that often a dark solution colors the paper and makes it hard to be accurate visually. The test strips where the color scale and the sample spot on the paper all get the same dunk and are effected equally by the color of the solution.
 
These test papers are excellent and the color scale is on each strip. If you need to be more precise they are available in short ranges for more precise determinations.

The advantage of the color scale on the test strip is that often a dark solution colors the paper and makes it hard to be accurate visually. The test strips where the color scale and the sample spot on the paper all get the same dunk and are effected equally by the color of the solution.
Awesome will have a look at the strips 👍
 