Hi friends,
I read in a Reddit thread that neither poor man’s nitric or poor man’s AR should be used when the goal is to refine to three nines or higher.

Is this true? What do these methods leave behind that won’t refine out?

I personally was planning on poor man’s nitric for some things and AP for others.
 
So why does everyone prefer AP over poor man’s nitric if poor man’s nitric is faster? Not that we’re trying to win a race or anything…
Poor mans Nitric means making it by mixing the Nitrate and the Sulfuric, then either freezing it and removing some of the salts and using it as is.
Or Distilling it and get pure acid.
When we use AP it is just straight forward and no need for extra steps, and it do not create Metastannic acid.
 