How do I separate gold from an alloy of Gold, Tin and Copper?
I am unable to recover the gold, require help please
I am unable to recover the gold, require help please
actionakash said:I have taken the pins of the computer connectors with gold polish and melted the metal mix to form an alloy. I have got the alloy tested and it shows 1% gold 29% tin and 70% copper. The tin seems to trouble me the most. I am unable to get rid of it.
:shock:actionakash said:I have taken the pins of the computer connectors with gold polish and melted the metal mix to form an alloy
There is no need to re-melt this and cast as shot or cornflake if it is truly an alloy of 1% gold, 29% tin, and 70% copper. HCl digestion will leave him with a very fine gold particulate that will need to be recovered from his solution with care however.Geo said:remelt, pour into shot or cornflake
Sure will just like AP, just slower to start.Geo said:will that deal with the copper too?