im new here to the fourm, but have been refining for a few years. i have bought a couple lots of gold filled jewelry off ebay and made some money, but i have always wondered about these types of listings?
http://www.ebay.com/itm/500-5mm-IMPRESSIVE-UNISEXS-SHINING-10KT-REAL-YELLOW-GOLD-FILLED-NECKLACE-/370588057872?_trksid=p3286.m7&_trkparms=algo%3DLVI%26itu%3DUCI%26otn%3D3%26po%3DLVI%26ps%3D63%26clkid%3D7141378697086498695
it says its a 10k filled necklace, and that it weighs 26grams, for $5.72 even if its 1/20 it can still be worth refining. and there are a lot of these types of listings, some with over 100 in stock.
and what im asking, is if it to good to be true?
http://www.ebay.com/itm/500-5mm-IMPRESSIVE-UNISEXS-SHINING-10KT-REAL-YELLOW-GOLD-FILLED-NECKLACE-/370588057872?_trksid=p3286.m7&_trkparms=algo%3DLVI%26itu%3DUCI%26otn%3D3%26po%3DLVI%26ps%3D63%26clkid%3D7141378697086498695
it says its a 10k filled necklace, and that it weighs 26grams, for $5.72 even if its 1/20 it can still be worth refining. and there are a lot of these types of listings, some with over 100 in stock.
and what im asking, is if it to good to be true?