Hi, had anyone tried using citric acid or sulphamic acid mixed with NaCl and O2 from air pump or H2O2 to remove base metals and leave behind gold foils ?
I got my hands on some 20-30% citric acid detergents and one with 10% sulphamic acid mixed with few% of citric, i've been running a test for 3 days so far with aquarium pump and from some boards the tin got removed in others copper started to very very slowly dissolve but saddly i had to disconnect the pump due to excessive foaming from other components of the detergents and i've been wondering if anyone tried anything similar since i'm now battling with thoughts should i add some defoamer or something, since i cant get any SDS on it and i don't know if it wouldnt mess up something.
Also maybe someone else tried this method and got some feedback
I got my hands on some 20-30% citric acid detergents and one with 10% sulphamic acid mixed with few% of citric, i've been running a test for 3 days so far with aquarium pump and from some boards the tin got removed in others copper started to very very slowly dissolve but saddly i had to disconnect the pump due to excessive foaming from other components of the detergents and i've been wondering if anyone tried anything similar since i'm now battling with thoughts should i add some defoamer or something, since i cant get any SDS on it and i don't know if it wouldnt mess up something.
Also maybe someone else tried this method and got some feedback