Using US silver coins to make karat gold...

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

evanJ

Member
Joined
Oct 25, 2024
Messages
17
Location
los angeles
Hi! I am approaching the last stages in my jewelry project, and am ready to produce 18 karat shot. I have about 27.5 grams of refined gold, and have settled on a "green gold" alloy described here as it should be the right strength and color I am looking for. Doesn't hurt that it calls for 9:1 Ag/Cu, which I happen to have a lot of in the form of US silver quarters and dimes!

Or so I thought... But when looking for evidence of this ratio of silver to copper, I couldn't find much proof beyond the claims of the US mint.
This is the only XRF I could find, which on page 6 lists the copper content at 12% and the silver content at only 82.5%

So I'm wondering...
  • Has anyone successfully made an alloy of 75% gold, 25% junk silver from US coins? If so, were its properties consistent with what you would expect from 9:1 Ag/Cu?
  • Do you know of XRF reports that prove the 9:1 ratio?
  • Or - has anyone recovered 90% silver and 10% copper and nothing else from US silver quarters and dimes? It's my understanding that even a little nickel or zinc will botch my alloy.
edit: I might add that I've also recovered enough silver from my refining to use instead, and that I don't mind buying a few cents worth of copper... but it would be really cool to use the junk silver if that doesn't botch everything.

Thanks so much!
Evan
 
Last edited:
To be certain, I would alloy with only known parts of .999 metals. To do so using Ag coin alloy could be a crap shoot. Ag content has varied through out our (US ) history. Do what you may, you are putting your stamp, and reputation on the line.
 
US war time nickels are only 40% Ag....I think 1941-1945.
Wartime nickel alloy was 56% copper, 35% silver, and 9% manganese. Part of 1942 through end of 1945.

Due to manganese, I would advise not using war nickels to make alloys for jewelry.

The document Dave linked to earlier shows composition of US coins. I have a similar, but much older, document in my files somewhere.

Also, the advice from nickvc to clean coins before use is good advice prior to any melt.

Time for more coffee.
 
I have a jar full of them, but I don't know what to do with them. I don't think they are worthy of processing yet and a lot of places aren't interested in them.
Send me a PM stating how many you have. I might be interested, depending on lot size. And no, they are not normally worth processing. Manganese tends to muck things up for me.

Time for more coffee.
 