eastky
Well-known member
The last pictures you posted that is gold on those wafers but they could also be a sputtering target. Do a search for platinum or gold or silver sputtering target.
I am going to ask you some questions and I am going to give you some tips. If some of the tips sound rude I am sorry that you took it that way. After you read this post stop what you are doing and thinking and just clean your mind and thoughts. That stuff isn't going to disappear over night.
These are questions to you to think about and don't be in a hurry to respond.
1 Do you have to remove the stuff asap or can you do it over a week? can it be left there for a month while you sort here it?
2 How big is the building and how much stuff is in it that matters? By (matters) means electronic components lab ware type of stuff. Wafers. How much is trash? bags papers pallets boxes and stuff that has no value.
They tips I will give you are as follows.
1 Slow down
2 Inventory things put all the same items together and post a picture of multiple items in one picture. Instead of 2 or 3 items in a picture making multiple post of pics.
3 Maybe you should put together a group items for sale as a donation to forum to to pay for all the bandwidth you are using posting so many pics. This is the important tip.
4 You seem to be posting a lot of pics of gold plated components. If you have components that are loose and not in a bag or box. Go buy some zip lock sandwich bags and bag them up. Any components that you see gold on goes in a bag or stays in the bag or box they are in and goes in a big box to be dealt with later.
5 Work in one area at a time. If you open it close it if its loose bag it box it up and move to the next area.
6 If they manufactured wafers there you need to be looking for sputtering targets. Did you get that????
That is the major money that is possibly in that building
I am going to ask you some questions and I am going to give you some tips. If some of the tips sound rude I am sorry that you took it that way. After you read this post stop what you are doing and thinking and just clean your mind and thoughts. That stuff isn't going to disappear over night.
These are questions to you to think about and don't be in a hurry to respond.
1 Do you have to remove the stuff asap or can you do it over a week? can it be left there for a month while you sort here it?
2 How big is the building and how much stuff is in it that matters? By (matters) means electronic components lab ware type of stuff. Wafers. How much is trash? bags papers pallets boxes and stuff that has no value.
They tips I will give you are as follows.
1 Slow down
2 Inventory things put all the same items together and post a picture of multiple items in one picture. Instead of 2 or 3 items in a picture making multiple post of pics.
3 Maybe you should put together a group items for sale as a donation to forum to to pay for all the bandwidth you are using posting so many pics. This is the important tip.
4 You seem to be posting a lot of pics of gold plated components. If you have components that are loose and not in a bag or box. Go buy some zip lock sandwich bags and bag them up. Any components that you see gold on goes in a bag or stays in the bag or box they are in and goes in a big box to be dealt with later.
5 Work in one area at a time. If you open it close it if its loose bag it box it up and move to the next area.
6 If they manufactured wafers there you need to be looking for sputtering targets. Did you get that????
That is the major money that is possibly in that building