Looks just like my turkey fryer burner made by KingCooker.While the foils may impress many, where did you get that pipe mounted gas burner?
It's a cheap emergency use replacement because I broke my main one. The quality isn't good at all but it does the job.While the foils may impress many, where did you get that pipe mounted gas burner?
You take the concept of cherry picking to a new level!It came out at 62g overall. 62g / 2.4 = 25.8g per Kg.
I've never particularly liked trying to dissolve lids in their entirety with ceramics. They take too long compared to the rest of the processor.You take the concept of cherry picking to a new level!
I always pop the lids off all the processors. And scrape as much of the indium off as I can too.I've never particularly liked trying to dissolve lids in their entirety with ceramics. They take too long compared to the rest of the processor.