gecekurdu42 said:white or black.
I am refining 400 grams ( little-big-zilog-white-black ) gold plated chips.
Finaly : 400 grams : 2.6-2.8 grams gold bottoms. And analiys % 91.50 gold, 22 krat.
Barren Realms 007 said:gecekurdu42 said:white or black.
I am refining 400 grams ( little-big-zilog-white-black ) gold plated chips.
Finaly : 400 grams : 2.6-2.8 grams gold bottoms. And analiys % 91.50 gold, 22 krat.
So you processed aproximately 60 chips with a yield of about .04g per chip. Nice