M Makayu_glass New member Joined Apr 2, 2013 Messages 3 Apr 16, 2017 #1 Hello every ? Any one familier with thé yield of these gold transistors and how to go about recovering golf from them ? Attachments IMG_20170411_215848.jpg 2.1 MB IMG_20170411_215743.jpg 2 MB
Hello every ? Any one familier with thé yield of these gold transistors and how to go about recovering golf from them ?
N nickvc Moderator Staff member Moderator Joined Sep 14, 2009 Messages 5,658 Location birmingham Apr 16, 2017 #2 I can't give you specific numbers but those parts are very good for e scrap, the white part is beryllium so care is needed when removing it to maximise the yield.
I can't give you specific numbers but those parts are very good for e scrap, the white part is beryllium so care is needed when removing it to maximise the yield.
g_axelsson Administrator Staff member Administrator Moderator Joined Nov 17, 2007 Messages 5,545 Location Sweden Apr 16, 2017 #3 According to datasheet the "Gold plating thickness: flange & leads: 1.14 ± 0.38 micron [45 ± 15 microinch]". http://www.infineon.com/dgdl/Infineon-PTFA091201EF_V4-DS-v03_01-EN.pdf?fileId=db3a30431c69a49d011c75bf826001ae Göran
According to datasheet the "Gold plating thickness: flange & leads: 1.14 ± 0.38 micron [45 ± 15 microinch]". http://www.infineon.com/dgdl/Infineon-PTFA091201EF_V4-DS-v03_01-EN.pdf?fileId=db3a30431c69a49d011c75bf826001ae Göran