Zinc Hydroxide

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

rickzeien

Well-known member
Joined
Nov 14, 2017
Messages
544
I got a quote today for almost 1400.00 for 1 Kg of 2N.

Any one have info on how to make my own.






Sent from my SM-G950U using Tapatalk
 
I’m not giving you a hard time, I’m just curious if you really need 2n certified or if you just need reagent zinc hydroxide. The latter can be prepared by precipitation of zinc dissolved in hcl, by sodium hydroxide.

Or if you are looking for zinc powder to precipitate Pgms or something.




Sent from my iPhone using Tapatalk
 
snoman701 said:
I’m not giving you a hard time, I’m just curious if you really need 2n certified or if you just need reagent zinc hydroxide. The latter can be prepared by precipitation of zinc dissolved in hcl, by sodium hydroxide.

Or if you are looking for zinc powder to precipitate Pgms or something.




Sent from my iPhone using Tapatalk
Doesn't need to be certified. It was the only one I found that had it to quote so far. That was the lowest grade they had.

I have everything I need to make it including PPE and a fume hood with a scrubber.

Thanks

Sent from my SM-G950U using Tapatalk

 