A
Anonymous
Guest
Edited to add UPDATE 01
Hello members,
I've been processing and refining silver from keyboard mylars nearly a month now with great success. Although I'm not finished with my own supply, I have the process down packed and if you need to have your keyboard mylars done for you, I will do it.
Here are the terms.
1. You pay to have the mylars shipped to me. I'll pay to have the silver shipped back to you.
2. A minimum of 4lbs of mylars. (that's approximately 2 ozt silver)
3. No carbon mylars (the ones that have black contact points).
4. We split the yield 50/50.
Once all the mylars are stripped and everything is cemented, I'll weigh it, then split the cemented silver in two portions, then melt the two separately, and whichever weighs the most after melting, I'll send that to you.
I will be pouring the silver in 1 ozt molds. If there is more than 5 ozt silver for you, I'll be pouring them in 5 oz conical molds (saves time from doing 1 ozt at a time). If you insist on them being poured into a particular mold, let me know.
It should take me no more than 3 days to do 4 lbs at most. You should have your silver in about 7 days from the time I receive them (longer for more than 4 lbs).
PM me if you have any questions or concerns.
Kevin
[UPDATE 01]
Please include your forum username inside of the package because someone else may have the same name as yours.
Hello members,
I've been processing and refining silver from keyboard mylars nearly a month now with great success. Although I'm not finished with my own supply, I have the process down packed and if you need to have your keyboard mylars done for you, I will do it.
Here are the terms.
1. You pay to have the mylars shipped to me. I'll pay to have the silver shipped back to you.
2. A minimum of 4lbs of mylars. (that's approximately 2 ozt silver)
3. No carbon mylars (the ones that have black contact points).
4. We split the yield 50/50.
Once all the mylars are stripped and everything is cemented, I'll weigh it, then split the cemented silver in two portions, then melt the two separately, and whichever weighs the most after melting, I'll send that to you.
I will be pouring the silver in 1 ozt molds. If there is more than 5 ozt silver for you, I'll be pouring them in 5 oz conical molds (saves time from doing 1 ozt at a time). If you insist on them being poured into a particular mold, let me know.
It should take me no more than 3 days to do 4 lbs at most. You should have your silver in about 7 days from the time I receive them (longer for more than 4 lbs).
PM me if you have any questions or concerns.
Kevin
[UPDATE 01]
Please include your forum username inside of the package because someone else may have the same name as yours.