kjavanb123
Well-known member
All,
I depopualted a batch of cellphone boards, weighed 955 grams, after depopulation they weighed 220 grams, I used my test pyrolysis ubit then mix the burned boards with equal part soda ash and borax, melt it and got 58.9 grams of copper.
Based on above, copper content in form of laminated in depopulated cellphone board is 26.77%.
I am trying to compile a list of copper content of different type of boards that I already depopulated and smelted.
Using a good pyrolysis, and a simple furnace, I am going to recover copper from the bare boards.
Regards
Kj
I depopualted a batch of cellphone boards, weighed 955 grams, after depopulation they weighed 220 grams, I used my test pyrolysis ubit then mix the burned boards with equal part soda ash and borax, melt it and got 58.9 grams of copper.
Based on above, copper content in form of laminated in depopulated cellphone board is 26.77%.
I am trying to compile a list of copper content of different type of boards that I already depopulated and smelted.
Using a good pyrolysis, and a simple furnace, I am going to recover copper from the bare boards.
Regards
Kj