bes8718
Active member
I'm not sure what voltage to run my silver cell at or how the voltage actually affects the cell.
The cell is set up in a 1 ltr beaker with 95g per litre of silver
The anode basket has muslin cloth as a filter
The cathode is a 45mm×12mm graphite block
I am feeding roughly 98-99% pure silver through it
Any information would be greatly appreciated
The cell is set up in a 1 ltr beaker with 95g per litre of silver
The anode basket has muslin cloth as a filter
The cathode is a 45mm×12mm graphite block
I am feeding roughly 98-99% pure silver through it
Any information would be greatly appreciated