S saadat68 Well-known member Joined Aug 7, 2016 Messages 482 Dec 10, 2016 #41 This is my last design! Can someone confirm it ? Is it OK ? Thanks
A autumnwillow Well-known member Joined Apr 1, 2010 Messages 450 Dec 19, 2016 #42 So many fittings, that probably costed you a lot, but you are already there. Test it yourself. I have provided the guidelines.
So many fittings, that probably costed you a lot, but you are already there. Test it yourself. I have provided the guidelines.
S saadat68 Well-known member Joined Aug 7, 2016 Messages 482 Dec 29, 2016 #43 autumnwillow said: So many fittings, that probably costed you a lot, but you are already there. Test it yourself. I have provided the guidelines. Click to expand... Thanks I wait for some connections I will add some images after finish it 8)
autumnwillow said: So many fittings, that probably costed you a lot, but you are already there. Test it yourself. I have provided the guidelines. Click to expand... Thanks I wait for some connections I will add some images after finish it 8)
S saadat68 Well-known member Joined Aug 7, 2016 Messages 482 Dec 29, 2016 #44 I want to destroy my scrubber! It is big ( 3 columns with 100 cm height ) and I fear put that in my workshop 3 columns full of NaOH I really fear Can I make 6 column ( each on 50 cm ) instead of three column ? I think it is safer :?
I want to destroy my scrubber! It is big ( 3 columns with 100 cm height ) and I fear put that in my workshop 3 columns full of NaOH I really fear Can I make 6 column ( each on 50 cm ) instead of three column ? I think it is safer :?
A autumnwillow Well-known member Joined Apr 1, 2010 Messages 450 Dec 30, 2016 #45 If the vacuum is working, just use supports to hold the vessels well and safety buckets for each.
S saadat68 Well-known member Joined Aug 7, 2016 Messages 482 Dec 30, 2016 #46 I destroy it I really fear. prefer to make a smaller one.