I run 338grams of gold plated ceramic lids through AR.I have recovered all but a little that is sitting in my decant pot(maybe 1-4 tenths of a gram.Does 10.3grams sound low or do you think I got it all.I will be doing a first refine on this button,because it has some slight contamination.The button still has borax from were I have not cleaned it yet.Thanks in advance.