Stirring in the presence of iron didn’t work for me. I still had agcl present.

I had to tumble the silver chloride with iron as the grinding media.

You need intimate contact between the agcl and the iron.


Sent from my iPhone using Tapatalk
 
snoman701 said:
...You need intimate contact between the agcl and the iron...
Well, I have a magnetic stirrer on the way to my house by tomorrow at 8pm, so we'll see if that works better than just hand-stirring everything around while it's reacting.
 
BSGMiner said:
snoman701 said:
...You need intimate contact between the agcl and the iron...
Well, I have a magnetic stirrer on the way to my house by tomorrow at 8pm, so we'll see if that works better than just hand-stirring everything around while it's reacting.

Yes that's a good start it does work better.

Jon
 
BSGMiner said:
snoman701 said:
...You need intimate contact between the agcl and the iron...
Well, I have a magnetic stirrer on the way to my house by tomorrow at 8pm, so we'll see if that works better than just hand-stirring everything around while it's reacting.
It didn’t work for me.

Short of preparing hard to dissolve solids, I do not find magnetic stirrers to be of great use in refining.




Sent from my iPhone using Tapatalk
 
snoman701 said:
...I do not find magnetic stirrers to be of great use in refining...
I'm going to try it for alternating HCl and H2O washes/rinses this weekend to see how that goes first.
 