No one can tell you anything based on pictures. Some pyrites contain precious metals, some do not. Only an assay will answer the question.
Dave
Dave
Welcome.Hello. Im from indonesia and im new here. I had with me 3 samples of pyrites. If any of you guys had good knowledge in pyrites, your comments is much appreciated.
Btw, I'm looking for gold or PGM if ever existed in these rocks.
Best Regards.
View attachment 58713View attachment 58714View attachment 58715
Welcome.
This is a forum for refining precious metals not for mining and ores.
With that said, there are some skilled "miners" in here so they might chime in.
Another thing is that even if pictures is nice it is next to impossible to identify something by pictures alone.
More information is needed.
XRF on ores are very prone to errors, best to get a proper assay.Thanks Yggdrasil.
I will get an xrf report soon. God's willing.