There will be no Silver if you used AR as Silver will form AgCl which is not soluble.
Anyway since you have not said at which pH you stopped the addition of NaOH we have no idea which hydroxides you have dropped
I didn't ask for the identification of my hydroxides. I asked for people to see if they recognize the pgm from my pictures. I am not a newbie and don't need help with my process. I'm just trying to see what pgm I have. That's all. Please see the pictures
 
The
He means brown is a reaction of copper chloride to stannous chloride. Called a false positive. To see if there is any purple(gold), dilute the test drop.
No copper was present. I tested 3 different times on different occasions and got the same color. Then I dropped the gray powder in the picture
 
I didn't ask for the identification of my hydroxides. I asked for people to see if they recognize the pgm from my pictures. I am not a newbie and don't need help with my process. I'm just trying to see what pgm I have. That's all. Please see the pictures
The pictures are useless.
Get your stuff tested with a XRF or an ICP or other spectral instrument.

We can not help more, since you are not willing to help us help you.
 
I have not said anything regarding Urea, even though we prefer Sulfamic acid.
And we do not call that neutralizing because that is to bring the solution to 7 which is neutral.
We call it deNOxing since we decompose the NOx to avoid re dissolution.

Red is probably colloidal Gold.
Add a splash of Peroxide into your HCl and it will dissolve.
Just that you will never see it since it is so small amounts.
Gold is not metallic silver color
 