Well I did a little experiment today, I tried to depopulate a ram stick in hot baby oil. I can’t be the only one to ever think of that but I haven’t seen it posted anywhere before so I tried it.
I figured all I needed was something that boils higher than the melting point of solder.
I’m sure there is a better oil, maybe olive or something but it’s reusable and the baby oil smells kinda good when hot. Just thinking outside the box as I’m finally getting ready to process @50 lbs of ram sticks and after the painstaking process of cutting off fingers I was looking for something cheap and effective.
I also tried dissolving bga chip in Ethylene glycol and a catalyst after reading a paper about it, I used sodium hydroxide but the paper was about TBD ? as a catalyst compared to other catalysts.
Anyway that didn’t work for me.
But the oil bath with a little agitation stripped chips but the solder will wick onto anywhere it can so if there are still fingers on the board the solder may flow there.
Just thought I’d post the info, commensurate flaming
:mrgreen:
I figured all I needed was something that boils higher than the melting point of solder.
I’m sure there is a better oil, maybe olive or something but it’s reusable and the baby oil smells kinda good when hot. Just thinking outside the box as I’m finally getting ready to process @50 lbs of ram sticks and after the painstaking process of cutting off fingers I was looking for something cheap and effective.
I also tried dissolving bga chip in Ethylene glycol and a catalyst after reading a paper about it, I used sodium hydroxide but the paper was about TBD ? as a catalyst compared to other catalysts.
Anyway that didn’t work for me.
But the oil bath with a little agitation stripped chips but the solder will wick onto anywhere it can so if there are still fingers on the board the solder may flow there.
Just thought I’d post the info, commensurate flaming