necromancer
Well-known member
hello all,
i am happy to say that i have recovered my first foils
a nice pile recovered from 386/486 kovar top & bottom plates only, there a little dirty right now but i will clean them up dissolve in AR & drop with SMB.
wash properly, dry & melt
thanks goes out to everyone here on the forum :!:
without you guys i would be getting $0.45 per pound
i have close to 20 pounds of cpu to process, that will be fun
i am happy to say that i have recovered my first foils
a nice pile recovered from 386/486 kovar top & bottom plates only, there a little dirty right now but i will clean them up dissolve in AR & drop with SMB.
wash properly, dry & melt
thanks goes out to everyone here on the forum :!:
without you guys i would be getting $0.45 per pound
i have close to 20 pounds of cpu to process, that will be fun