hello can someone know if i can use aqua regia in 0.81% of gold purity direct to aqua regia solution
for refining process
best regards.
 

Attachments

  • 2014-03-14 13.33.05.jpg
    2014-03-14 13.33.05.jpg
    88.3 KB
If it is 81% gold it should go ok in AR maybe not the cleanest dissolution but it should dissolve.
If it 0.81% no chance for AR you need to discover the base metal contaminants before anything else.
 
If it is 80+ percent gold it may have silver too high for effective attack with aqua regia. To be on the safe side, inquart with silver and part in nitric, then aqua regia on the remaining gold should be very easy and yield high purity gold.
 