D Drowningbodacius Well-known member Joined Sep 12, 2012 Messages 68 Location P-town, Virginia Sep 25, 2012 #1 i was wondering if there was a chem beth of some sorts i could dissolve tin solder off of PCB??
Palladium Well-known member Joined Jan 17, 2008 Messages 5,724 Location USA Sep 25, 2012 #2 A good soak in straight hcl.
D Drowningbodacius Well-known member Joined Sep 12, 2012 Messages 68 Location P-town, Virginia Sep 25, 2012 #3 thanks Palladium for the quick response. i know muratic acid is the same as hcl s i could use that as well right?
thanks Palladium for the quick response. i know muratic acid is the same as hcl s i could use that as well right?
Palladium Well-known member Joined Jan 17, 2008 Messages 5,724 Location USA Sep 25, 2012 #4 Yes Muratic and hcl are the same. Sort of like H20 and water is the same thing just a different name is all.
Yes Muratic and hcl are the same. Sort of like H20 and water is the same thing just a different name is all.
D Drowningbodacius Well-known member Joined Sep 12, 2012 Messages 68 Location P-town, Virginia Sep 25, 2012 #5 lol thats what everyone keeps tellin me lol thanks again palladium