Hi everyone.
First off I'm in Canada. I've selected what seems to be my best option here to send my gold fill for refining. I hope you folks can answer a few questions before I take the leap?
I have about 7000 grams (about 225 ounces) of wrist and pocket watch super clean material. It is 1 tenth 12k typically or better. I have stripped 99 percent of any magnetic material.
That said here's the questions:
They offer 90% on the yield. Can I do better?
They say.they will simply burn it then melt it. Am I losing a significant portion of gold in this process? Is there a better method I should be looking for?
What would my expected yield be?
BIG thank you for your expertise guys!
Rod
First off I'm in Canada. I've selected what seems to be my best option here to send my gold fill for refining. I hope you folks can answer a few questions before I take the leap?
I have about 7000 grams (about 225 ounces) of wrist and pocket watch super clean material. It is 1 tenth 12k typically or better. I have stripped 99 percent of any magnetic material.
That said here's the questions:
They offer 90% on the yield. Can I do better?
They say.they will simply burn it then melt it. Am I losing a significant portion of gold in this process? Is there a better method I should be looking for?
What would my expected yield be?
BIG thank you for your expertise guys!
Rod