A Anonymous Guest Mar 14, 2010 #1 what strength does hydrochloric need to be to make (AR) I can get hold of 32% strength hydro and get hold of 70% strength Nitric
what strength does hydrochloric need to be to make (AR) I can get hold of 32% strength hydro and get hold of 70% strength Nitric
J jimdoc Well-known member Joined Mar 12, 2007 Messages 4,943 Location Philadelphia Mar 14, 2010 #2 That will work. Jim
A Anonymous Guest Mar 14, 2010 #3 thanks Jim , am just about to go to the shed and melt some refined silver that I dropped out of 70% nitric with copper tubing