I saw a vevor electric with 1kg and 3kg crucible. I have 12-14k little pieces. Want to pour a bar. Will it still be 12 to 14k. Ir is it easy to separate the gold. The refining places seem like a waste of time. Their website say the do personal orders. But when you talk them they aren't invested in the business, they just want large quantities from company's and businesses. I figure I have lots of time to learn. I don't mind making mistakes and losing money. That's how you learn. Thought a couple hundred buck fir an electric setup was a good starting point and once I get a feel for it and learn more can invest more into a better system.You'll need to give a little more information to get good advice. Are you talking about the little electric type, propane or gas fired, etc? How large a furnace are you looking for, like how much do you intend to melt at a time? Do you want to melt gold, silver, other?
Dave
Never heard of inquartation. Thanks for the advice will research those units. Not is a rush. Want something for the new year. I would do small batches. Dont want the bars bigger then 10 ounces. Kinda have the option to do 1 or 10 ounce pieces roughly. 100 ounce or 1 kilo bars I don't want that much in one bar. I don't mind if it stays 12k-14k but would like to learn how to separate. I just don't get how it all pours out and doesn't stick to the inside of the pot. Like, if you pour a glass of cream, the glass will be empty be still lined with cream. Sorry if that is a bad example. Just a young guy learning.One thing to be careful with the small resistance heat furnaces is capacity. They rate the crucibles for 1 kg of pure gold, which is half a kilo of silver and a little more than half a kilo of mixed karat. So capacity, and the fact that they don't last very long and the crucibles are pricey would steer me towards a propane furnace. A furnace that holds a #2 bilge crucible will be good for smaller melts and serve you well as you scale up to refining. They are also quite reasonably priced and if you want to get into refining and what you refine is jewelry related, remember if you use inquartation, which we highly recommend, you need crucible capacity to inquart.
After you have melted the scrap it has no markings anymore and can not be sold as is.I saw a vevor electric with 1kg and 3kg crucible. I have 12-14k little pieces. Want to pour a bar. Will it still be 12 to 14k. Ir is it easy to separate the gold. The refining places seem like a waste of time. Their website say the do personal orders. But when you talk them they aren't invested in the business, they just want large quantities from company's and businesses. I figure I have lots of time to learn. I don't mind making mistakes and losing money. That's how you learn. Thought a couple hundred buck fir an electric setup was a good starting point and once I get a feel for it and learn more can invest more into a better system.
After you have melted the scrap it has no markings anymore and can not be sold as
ThMany forum members started with very little to no experience. A few have went on to become large scale and some stayed small scale. And a few decided it wasn't for them and moved on. So if you need to learn here is the place to do it. Welcome to GRF.
Thank. I think it is a good skill set to have. Even making copper bars would be nice. I can see copper going way up in time. And silver I always knew would take a big jump. Alot easier for silver and copper to double, but $6000 an ounce for gold I can't see. But no expert. When your melting it does it need a certain temp is too hot no good?Many forum members started with very little to no experience. A few have went on to become large scale and some stayed small scale. And a few decided it wasn't for them and moved on. So if you need to learn here is the place to do it. Welcome to GRF.
My hobby of Hydrometallurgy started when I was 10 years old In Northern Rhodesia. My first melting furnace is now called " Flowerpot Furnace" It uses Charcoal and a bellows ( Hair dryer fan) The Local Indigenous people have used this furnace to melt Iron, since the Iron Age. It is easy and Cheap, Cheap!As Yggdrasil said, once melted into a bar, the markings are lost and the value is decreased. You can increase the value by purifying it and then sell it to a refiner who will pay you a percentage of the value minus their cost to confirm purity and purify to their standards. You will be able to recover the silver (often an alloy of 12k and 14k).
If you are determined to "make a bar" before you start refining, I would separate the like karat scrap and melt the lots individually, stamping the resultant bar for your own reference. You will not purify or the refine gold at this stage. You are simply melting jewelry into indeterminate pieces of metal.
If you want to start refining, you can add silver to save the gold as 6K inquarted gold. The calculations are not complicated but a mistake can cost time and reagents later.
You do not need a furnace to melt karat scrap. An appropriate propane torch will work if the melt dish is insulated. A MAPP or propane/MAPP with oxygen is quicker. If you have an oxy/acetylene torch, don't bother with propane.
Just my .02
SRM
Welding shop with hood. That's why I want to figure out the borax. I don't mind handling lead but would like to avoid it. I mean at 12-14k nothing wrong with just pouring a 12-14k bar. I see 10k bars all the time. I grew up with with the old man building house and lots of wood working, my craft is working with wood. About 15 years ago I made friends with an old machinist. Brilliant man and learn a lot about steel, all the different types what is good for what and what is not good for certain things. Engineering always fascinated me. This just s like the next stepping stone for my wealth of knowledge. I respect anyone who works with metal or body shop so cold heavy and dirty. Everything about it is just dark. Wood is alive warm and bright. And would can be heavy but no one slings more weight then a metal worker. Everything about it just breaks the body.You do realize that when you use lead for cupellation about 10% of the lead volatilizes into the air. If you are doing this in a hood with good exhaust and possibly a bag house, no problem, but if you are doing this in the back yard upwind it is worth considering.
How about learning to swim before you dive from the deep end.I have seen a guy shape a bowl with Portland cement. He added three times the wight of the scrap gold and just melted it with a torch, the cement cupeled all the lead and impurities and was left with a nice button. I see a half dozen of cupels cost 45 bucks each one can absorb 300 grams of lead. I have .999 gold filled granules from refining that test between 12-14k. I figure I could refine 62 grams of granuals with 180 grams of of lead for each cupel. Then put the the button is a crucible. I know guy have been telling other methods. But this is in my comfort zone and I understand it. Acids I am not interested in, especially boiling them for hours. I like the borax method but haven't found a good video. Don't get how much to use. I know too much can dissolve the gold from what I have seen.
999 is close to 24k, 12k is 500I have .999 gold filled granules from refining that test between 12-14k