• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

AP Direct Clarificatoon Request - 2 Items

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Joined
Mar 1, 2025
Messages
5
Location
Calgary, Alberta
I have researched the AP method extensively and have been successfully utilizing it; however, I have two questions that I have been unable to find a definitive answer on:

1) Too much H2O2 can cause gold to dissolve into the AP solution, so an air bubbler is suggested. To speed things up, shoild I run the my air bubbler the entire time, or just once the solution heavily darkens and it needs to have oxygen added to bring it back to its emerald green color? If the air bubbler is run the whole time, can it cause the gold to dissolve into the solution? Logically it seems like running it the whole time would cause this, as the air bubbler adds O2 in place of the peroxide.... and too much peroxide = too much oxygen = dissolving gold.

2) Will heating the AP solution speed up the process, or not a material amount, and/or irs a bad idea due to ________?

Everything is done safely on my end and I have had numerous successful AP runs + have saved my solution and continue to successfully reuse it.

Thank you!
 
I have researched the AP method extensively and have been successfully utilizing it; however, I have two questions that I have been unable to find a definitive answer on:

1) Too much H2O2 can cause gold to dissolve into the AP solution, so an air bubbler is suggested. To speed things up, shoild I run the my air bubbler the entire time, or just once the solution heavily darkens and it needs to have oxygen added to bring it back to its emerald green color? If the air bubbler is run the whole time, can it cause the gold to dissolve into the solution? Logically it seems like running it the whole time would cause this, as the air bubbler adds O2 in place of the peroxide.... and too much peroxide = too much oxygen = dissolving gold.

2) Will heating the AP solution speed up the process, or not a material amount, and/or irs a bad idea due to ________?

Everything is done safely on my end and I have had numerous successful AP runs + have saved my solution and continue to successfully reuse it.

Thank you!
Welcome to us.
Well the AP name is kind of misleading since you do not need Peroxide at all.
HCl and some Copper and air bubbling is all that is needed.
If you find some green Copper it will start faster.
This leach is actually a Cuprous Chloride etch.
The reason for the naming is that in the beginning one used weak Peroxide as source for the Oxygen in stead of bubbling air through it.
And the name kind of stuck.

And yes some heat will make it faster.

Here are some links to study:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/threads/library-index-thread.22351/post-233795
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/library-index-thread.22351/post-233794

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.35743/

Video section: https://goldrefiningforum.com/threa...our-visual-learning-members.35185/post-379931

List of abbreviations: https://goldrefiningforum.com/threads/a-glossary-of-common-terms.21242/post-219169

Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 
Welcome to us.
Well the AP name is kind of misleading since you do not need Peroxide at all.
HCl and some Copper and air bubbling is all that is needed.
If you find some green Copper it will start faster.
This leach is actually a Cuprous Chloride etch.
The reason for the naming is that in the beginning one used weak Peroxide as source for the Oxygen in stead of bubbling air through it.
And the name kind of stuck.

And yes some heat will make it faster.

Here are some links to study:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/threads/library-index-thread.22351/post-233795
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/library-index-thread.22351/post-233794

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.35743/

Video section: https://goldrefiningforum.com/threa...our-visual-learning-members.35185/post-379931

List of abbreviations: https://goldrefiningforum.com/threads/a-glossary-of-common-terms.21242/post-219169

Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
Thank you for the response. I am aware that Peroxide is not actually needed and haven't used it since my 1st batch quite a while ago. However, I have just used my air bubbler intermittently since then to get the solution back to emerald green - in my question I was asking if constant bubbling would dissolve the gold into the solution? I've never run my bubbler the entire time due to not having/being able to find clarity on this particular item.

Thanks again
 
Thank you for the response. I am aware that Peroxide is not actually needed and haven't used it since my 1st batch quite a while ago. However, I have just used my air bubbler intermittently since then to get the solution back to emerald green - in my question I was asking if constant bubbling would dissolve the gold into the solution? I've never run my bubbler the entire time due to not having/being able to find clarity on this particular item.

Thanks again
Many years ago I started and did not use air bubbler for my first batch or two.
Also I used peroxide 3%.
Then I soon found out to use air all the time and just HCl.
Also if peroxide is/was used and after time much copper in solution the gold will precipitate out in its powder form.
It is then collected in filters, powder and foils.
The air is needed to oxidize the copper layer under the gold foils and the HCl will dissolve the layer of oxidized copper and nickel.
Its a slow reaction but works very well.

It is stated that gold will dissolve in HCl and an oxidizer.
That tells me some gold will dissolve.
It is a very slow process.
I always no matter what filter the solution when done, personally a couple times.
Losses are very minimal.

This leads also to, after storage of AP solution and waste handling.
You can still filter solution after much time of storage.
Possibly a small amount of what was fine gold powder has finally sat and stuck on the bottom of the bucket can be retrieved.
Use iron bar stock to get your copper and lower reactive metals.
Process copper in electrolytic cell and get some tiny amount of precious slimes.
its a long cycle of process but very interesting to follow.
 
Thank you for the response. I am aware that Peroxide is not actually needed and haven't used it since my 1st batch quite a while ago. However, I have just used my air bubbler intermittently since then to get the solution back to emerald green - in my question I was asking if constant bubbling would dissolve the gold into the solution? I've never run my bubbler the entire time due to not having/being able to find clarity on this particular item.

Thanks again
No the bubbling will not dissolve Gold.
But should be on all the time to rejuvinate the solution.
 
All HCl requires is an oxidizer to dissolve gold. The oxygen in the air is sufficient. The air dissolves into the HCl, and the gold can dissolve.

Dave
No the bubbling will not dissolve Gold.
But should be on all the time to rejuvinate the solution.
Ygg,
Yes apparently HCl and air can dissolve gold. How much? Most likely a very slow process.
See Frugals post above.
Also searches on the internet explain it.
 
It will dissolve some gold using an air bubbler. It just won't stay in solution with the copper and will precipitate out as a fine brown powder. I always left it and targeted the foils until I was ready to dispose of the AP. At that point I filtered everything out before disposal. I did this on my own material so the little bit that stayed in solution wasn't a loss to a customer.
 
I have never used the AP method because, quite frankly, for a commercial application it is too slow. However from a chemical perspective the air bubbler will provide oxygen to the solution to a point where the solution will not gain any more oxygen from the bubbles, (even as the bubbler continues to bubble away) it will reach a point of saturation. If some gold does dissolve it will quickly cement itself out anyway.
The peroxide on the other hand is a super oxygenated liquid which can bring the solution to over saturation and cause more gold to dissolve. Again depending on how much gold dissolves, which is controlled by the oxygen levels and the temperature, the copper levels will cause the gold to be cemented eventually. But if peroxide strengths are too high you may be assuming the gold has been de-plated and the solution is barren and it may not be true.

That is why testing the solution is important. If testing is too difficult, stick to air bubbles and be patient.
 
Last edited:
The chemists will tell you that HCl does not dissolve gold which is true, sort of , but as you are using the acid exposed to air it can and will dissolve some and other factors such as what else is in the solution come into play , the losses should be minimal and should be recovered via the stock pot or by reusing any HCl wash solutions of gold powder as the base for the next dissolution.
I’m with 4metals the whole AP process for a commercial refiner is too slow so I never used it but it does have a place for the hobby/ amateur refiner as a low cost and available alternative to the processes which the professionals use , often a cyanide based process.
 
No the bubbling will not dissolve Gold.
But should be on all the time to rejuvinate the solution.
This is very useful as I'm very close to starting a test batch of satellite SIM cards I've prepared. If goes well, a Gold forum donation will come from recovery profits as I appreciate the expert advice. Sorry, what is the forum protocol? To continue on from ShielaMartin780s blog or start a new one?
 
Sorry, what is the forum protocol? To continue on from ShielaMartin780s blog or start a new one?
It is done both ways, you can post on this thread or start your own. As you may have noticed from searching the forum it is important to title your thread in a way that reflects the topic as this allows members to search more effectively.

Welcome to the forum
 
This is very useful as I'm very close to starting a test batch of satellite SIM cards I've prepared. If goes well, a Gold forum donation will come from recovery profits as I appreciate the expert advice. Sorry, what is the forum protocol? To continue on from ShielaMartin780s blog or start a new one?
Be advised that much/most of the values may be inside the tiny chip.
 
It is done both ways, you can post on this thread or start your own. As you may have noticed from searching the forum it is important to title your thread in a way that reflects the topic as this allows members to search more effectively.

Welcome to the forum
Thanks, best start a new thread perhaps under "SIM recovery E-waste" so it's referenced for others
 