VolkD
Well-known member
Then I'm very lucky, I manage to get a 25kg bag here for just under €100.Here in the UK Sodium Persulfate starts at around £5 for 100g, so quite a considerable expense compared to £15 for 5L of HCl to make CuCl2 which can perform dozens if not hundreds of etches.