VolkD
Well-known member
Back to topic:
Today I made a solution of 0.5l water + 100g sodium persulfate + bubbles. I put about the same amount of printed circuit boards in the solution. The etching process started at 9:15 local time, and ended around 19:30 local time. Then another two hours of filtering. The process with sodium persulfate alone is therefore slower than the one with acid.
Today I made a solution of 0.5l water + 100g sodium persulfate + bubbles. I put about the same amount of printed circuit boards in the solution. The etching process started at 9:15 local time, and ended around 19:30 local time. Then another two hours of filtering. The process with sodium persulfate alone is therefore slower than the one with acid.