• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Chemical Ap process question

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

bswartzwelder

Well-known member
Joined
Oct 24, 2011
Messages
660
I have read that as long as you bubble air into your AP solution, it can be rejuvenated forever or at least quite a long time. If AP is dissolving base metals and leaving the gold behind, aren't the base metals being dissolved using up the AP solution? I am basing this on the fact that a give amount of acid can only dissolve a given amount of metal. Once the acid is used up, or saturated with base metals, how can it continue to work? If it isn't the acid that's being used up, but is the hydrogen peroxide, won't it also reach a saturation point? I know you guys have the answers. Thank you in advance.
 

Latest posts

Back
Top