AP Recipe - How to make

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Silverfox: As to your post of November of '08.........

I am confused. I was under the impression that AR was 1:3 or 4 / nitric over HCL.. You mention using peroxide instead of HCL. Please explain. Phill
 
Jimdoc: Thank you much. I have it straightened out now. Phill

P.S. Have you seen the Geus website on the method from the Phillipines ? Tried it last night. IT WORKS !!!!!!!!!!!1
 
Possibly he is refering to the "Borax Method" of extraction found at this website?

http://www.geus.dk/geuspage-dk.htm?http://www.geus.dk/program-areas/common/geus_rep_2007-35-dk.htm
 
I really like the blowtorch! (and the idea of not splashing mercury around the mangrove)

But I can't quite figure out how the blowtorch is used.

There are two hoses from the "carburettor" to the burner, but only one of these have a valve? (the one terminating in the mesh)

Is the drawing incomplete?
 
I only have 16-19% Hcl available. Can I still use it in 4:1 ratio or should I put (6-8):1 ratio in my case.
Thank you
Platdigger said:
Muratic is generally around 31 percent.
It is not critical.
Randy
 
sad said:
I only have 16-19% Hcl available. Can I still use it in 4:1 ratio or should I put (6-8):1 ratio in my case.
Thank you
Platdigger said:
Muratic is generally around 31 percent.
It is not critical.
Randy

You can use the same ratio.The only 2 things:
1.When you see a gray mud start adding more muriatic.
2.Put an air bubbler(as that for the fishtanks) to compensate adding peroxide to your solution,after the initial start(3:1 HCl:H2O2)
 