giahylxag
Well-known member
That was my first purchase before coming to this forum, I planned to pre-mix AR before dropping to to gold, with the new AR mixing method I wont use it.I can se one thing you should not use, Urea.
You should either not overuse the Nitric or use Sulfamic Acid to DeNox your solution.
Make your AR like this: Cover the material HCl and then add Nitric in small increments until all Gold is dissolved.
For your Cupric Chloride leach, take some small Copper pieces and moisten them in HCl and let them sit until they are green.
When you start your leach, add HCl and wash the green Copper into it, then let an aquarium bubbler bubble air through it.
This will remove the Copper traces under the Gold foils.
Me and my partner is debating whether to use SMB, ferrous sulfate ot SO2 for dropping gold. Given what you said SMB is more effective, how about SO2 as 4metals suggest? I have read practices from the Germans and they use SO2 for dropping gold, the method "seems fast and clean" in my opinion. In my country, as far as I know we commonly use ferrous sulfate.It is better to use SodiumMetaBisulfate (SMB) for dropping the Gold, more effective.
Yes it is for waste treatment. The whole project will collapse if I can't treate waste and fume probably. I am living in the city center.Sodium Hydroxide won't be needed until your waste treatment.
Last edited: