D dmarth10 Well-known member Joined Aug 11, 2008 Messages 53 Location pennsylvania Oct 26, 2008 #1 I was wondering when recovering pgms from cats, what is the percent of typical recoery. Is it about 90-95%?
I was wondering when recovering pgms from cats, what is the percent of typical recoery. Is it about 90-95%?
S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 26, 2008 #2 http://www.goldmineworld.net/Aquaregia.html this enough?