R Renaldas Well-known member Joined Jun 16, 2009 Messages 99 Jul 25, 2010 #1 Who can write full chemical equation of gold chloride solution reacting with SMB? What are the other products except gold? NaCl, water, SO2?
Who can write full chemical equation of gold chloride solution reacting with SMB? What are the other products except gold? NaCl, water, SO2?
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida Jul 25, 2010 #2 Hopefully this is what you want: Gold Reactions Equations Steve