Moo

Well-known member
Joined
May 6, 2012
Messages
173
I have some foils in solution using hcl/bleach they have been sitting for about 20 hours however I have since produced more can I add these and a touch more bleach then wait another 24hrs and then precipitate?
 
Im sure someone alot more experienced then me can answer this better. You can add two solutions together, i would use litmus paper to determine acidity and go from there. Though I cant say cause i never make more then one batch at a time
 
sure, add those foils to your solution ,add a little heat and you might not even need to add chlorine to your solution. if it dont work with heat add a little hcl and a little javel (no much will be needed)
 