Ayham Hafez
Well-known member
I was sure that urea is not the best way to denox nitric, but I used it since sulphamic acid is not available in my country, but recently I had a bad experience with urea،I read that urea reaction with nitric is only generate H2O, but I think its much complicated since in my case it seems to react with other metals in dirty aquaregia solution and stop the work of SMB and ferrous sulfate, my advice for all is STOP USING UREA AT ALL!