boards with lots of gold pins

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

arthur kierski

Well-known member
Joined
Feb 10, 2008
Messages
1,130
Location
são paulo---brazil
does anyone know the yeald(aproximate) of gold from a kilo of this board?.
tomorrow i will receive 100kilos of these boards
the foto i am sending i obtained with the help of barren realm---thanks barren
 

Attachments

  • foto----compinosdorados-2aaa.JPG
    foto----compinosdorados-2aaa.JPG
    16.5 KB
Its contingent on too many variables.....the manufacturer,whether the pins are fully(or selectivly)plated,tel-com or mil-spec,how thick the pcb is,how many pins,how thick are the pins,how long.....etc.Its just too hard to tell arthur.
 
mic,they are full plated and the pins goes from one side to the other of the board(both sides,front and back)-----they are from telecon stuff and i obtained (blinded --by foto) 100kilos for 1500dollars(15dollars per kilo)-----that is all that i can tell you because i will receive these only boards tomorrow
thanks
Arthur
 
If the boards are not very thick then it sounds like you did good.
If the boards are very thick,then you will have a lot of scrap PCB material per kilo,and not many pins.I hope they are not very thick.
 
from107 kilos of these boards,i obtained 59grams of gold---that is 0,55grams of gold per kilo---i obtained this in 2days with gold strip leaching
i am sending these details for reference to forum members

Arthur Kierski
 
Hi arthur,
your yields sound a bit low per kilo,but like I said it depends a lot on the thickness of the boards.Were these boards quite thick?
Either way you ended up with a nice profit,good job bud.
J
 