Palladium said:Silver Refining Experiment Magnetohydrodynamics (MHD) :wink: :wink: :wink:
Martijn said:Nacho, i just read in another post that glass can break from the force of growing silver crystals if they get too thick inside the glass.
Put the cell in a catch basin in case of a spill.
Martijn said:Slow but steady @ 1.03Volt. Taking the time to grow slowly.
Martijn said:This is with the 250g/l silver concentration?
The cell back to work
of course, my girlfriend is already the owner of both crystals
Martijn said:I'm surprised to see so many fine coral grew in that little time.
Martijn said:In your cell i think the high concentration must be what's causing such growth at 0.2Volt.
I read in another thread that the concentration will level itself out if too low or too high. So that might just be the 'excess' silver coming out.
I suggest lowering the concentration to just below the recommended level and watch the first crystals grow at