Mica shist most likely. If the dust is black then maybe graphite. Shist is most likely if its flaky.
It's flaky but the dust that comes off it isn't black at all def. Not graphite and and it's so shiny it damn near mirrors you when you look at it don't think it's mica
 
You mean weight when you say gravity ?
The ratio of the density of the rock (in water) divided by the density of water. It has more applicability in identification if you are dealing with a single crystal. If you are going to do this with this rock, I would suggest breaking off a small piece to test. Once you are done with the small piece, crush it to a powder, pan it, and see what the heavy concentrates look like.

Other tests include hardness and streak, but most geologists will use a hand lens (7x-10x), look for rock and mineral types and identify the rock based upon the observation. From your description it sounds like the shiny stuff is muscovite mica, but it wouldn't be the first time I have been wrong.
 