i just saw in u-tube a process of cementing gold from computer parts from ar with magnesium foil-----in the video ,one sees the yellow gold powder and i noticed that cementing happened without elimination of nitrics---
please could some members coment this facts?
i cemented rh from rh sulphates spent solutions with magnesium and it worked very well
thanks all,
Arthur
 
Magnesium is higher on the reactivity list than even aluminum. All the other base metals in solution would cement. Very effective but a dirty choice.

I expect your Rh solution was reasonably clean to start with.
 
qst42know said:
Magnesium is higher on the reactivity list than even aluminum. All the other base metals in solution would cement. Very effective but a dirty choice.

I expect your Rh solution was reasonably clean to start with.



Hmmm interesting. Even more so since I still have a 110 pound drum of finely powdered magnesium I don't know what to do with. I used to sell a few chemicals to fellow fireworks enthusiasts, but they were much more interested in magnalium not magnesium.
 