Check out my progress so far

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

icejj

Well-known member
Joined
Feb 19, 2021
Messages
114
Decided to post this for anyone who'd like to see, and/or to provide some encouragement to the small-time hobbyist such as myself... this is most of what I've accumulated so far after about 3 years of recovery and refining.
 

Attachments

  • 20240403_164403.jpg
    20240403_164403.jpg
    918.4 KB · Views: 2
  • 20240403_164345.jpg
    20240403_164345.jpg
    765.8 KB · Views: 1
its way more than I have done.
You'll get there! Just keep trying and putting in the effort and it'll pay off.
Actually, its quite smart to store it in this format. A burglar will not understand its gold. But not in an instant coffee box. Then it might go in the bag.
Yeah that's one of the main reasons I store it this way. Another reason is that refining is quicker and requires less acid when dissolving precipitate vs a bar, just in case I want to do an additional refining.
 
Decided to post this for anyone who'd like to see, and/or to provide some encouragement to the small-time hobbyist such as myself... this is most of what I've accumulated so far after about 3 years of recovery and refining.
I “need” more patience! That looks real good. Looks like partial remedy for gold fever! Great work icejj
 
I'd guess somewhere between 2 and 4.
One thing I learned from seeing piles of dried powdered gold is to never guess what it weighs. I was always wrong because it shrinks so much when you melt it. Same was true when someone would see the gold remaining after parting an assay and ask me for a number.

Now melted gold is different, my guesses were closer!
 