4metals Moderator Staff member Supporting Member Moderator Joined Apr 5, 2009 Messages 7,004 Location northeast USA Jun 13, 2014 #22 Most of the ceramic chips I have worked with are a aluminum oxide mix which is the white ceramic looking base the circuitry is printed on. When ground up they looked like the pile you showed, fine white dust.