Copper(II) Chloride is highly soluble in water and will produce a blue solution, but when concentrated the CuCl2 aqueous solution will turn dark green.
 
aflacglobal said:
Copper(II) Chloride is highly soluble in water and will produce a blue solution, but when concentrated the CuCl2 aqueous solution will turn dark green.

Some Co2+ salts can be blue - but not CoCl2
So it should be CuCl2
Simple test is - add NaOH, and if precipitate is blue - and with ammonia produced dark blue solution - it's CuCl2
 