Around 5% I would expect, at least that fits the definition of hard lead.

But Rotometals carries it up to 30% antimony, more for blending custom bullet alloys.

http://www.rotometals.com/Antimony-s/1.htm

The link from Rotometals has a more complex ratio for clip on wheel weights.

http://www.lasc.us/SuperHard.htm

2% Sb and 0.5% Sn plus a trace of arsenic (As).
 