Wilton David

Member
Joined
Mar 6, 2025
Messages
6
Location
ECUADOR
Hello everyone, greetings from Ecuador, my English is not good and I use a translator to learn more about this forum, my question is how can I make my silver cleaner? I have around 800 grams and I mixed it with nitric acid which has a blue color and my question is what can I do to make it come out better quality, thank you very much for your comments.

The method I use is to add salt (sodium chloride), stir well with a wooden tube and wait for it to settle, pour out the acid and I am left with a white material that is like cheese, then I add floor shavings that replace the steel or aluminum nails and I proceed to dry and melt in fire, but I would like to improve the quality of my silver, thank you for your time.
 
Hello everyone, greetings from Ecuador, my English is not good and I use a translator to learn more about this forum, my question is how can I make my silver cleaner? I have around 800 grams and I mixed it with nitric acid which has a blue color and my question is what can I do to make it come out better quality, thank you very much for your comments.

The method I use is to add salt (sodium chloride), stir well with a wooden tube and wait for it to settle, pour out the acid and I am left with a white material that is like cheese, then I add floor shavings that replace the steel or aluminum nails and I proceed to dry and melt in fire, but I would like to improve the quality of my silver, thank you for your time.
To improve quality use pure Zinc, Aluminum or Iron.
Wash well when you are done converting it.
What kind of acid do you use?

Edit for thick fingers
 
Last edited:
Hello everyone, greetings from Ecuador, my English is not good and I use a translator to learn more about this forum, my question is how can I make my silver cleaner? I have around 800 grams and I mixed it with nitric acid which has a blue color and my question is what can I do to make it come out better quality, thank you very much for your comments.

The method I use is to add salt (sodium chloride), stir well with a wooden tube and wait for it to settle, pour out the acid and I am left with a white material that is like cheese, then I add floor shavings that replace the steel or aluminum nails and I proceed to dry and melt in fire, but I would like to improve the quality of my silver, thank you for your time.
Welcome to us by the way ;)
 
Last edited:
Para mejorar la calidad utilice Zinc, Aluminio o Hierro puros.
Lávelo bien cuando haya terminado de convertirlo.
¿Qué tipo de ácido utilizas?

Edición para dedos grues
To improve quality use pure Zinc, Aluminum or Iron.
Wash well when you are done converting it.
What kind of acid do you use?

Edit for thick fingers

Nitric acid 68%
Thank you for taking the time to answer me.
What type of zinc are you referring to? Can you attach an image?
 

Attachments

  • descarga.jpg
    descarga.jpg
    5.7 KB
That will be the next step.
When he has had a good clean conversion from Silver Chloride.
Probably would have been better to cement on Copper in stead of going via Silver Chloride.
I really appreciate your time and information

I know that it is better with silver chloride but where I live there is not much information and the method used is Merrill Crowe.
After putting and melting in the clay crucible, the material comes out in bars and we shot blast it and then we add nitric acid
and from there the silver comes out.


Edited quote to actually quote, and moved answer out of quote.
 
Last edited by a moderator:
I really appreciate your time and information

I know that it is better with silver chloride but where I live there is not much information and the method used is Merrill Crowe.
After putting and melting in the clay crucible, the material comes out in bars and we shot blast it and then we add nitric acid
and from there the silver comes out.


Edited quote to actually quote, and moved answer out of quote.
Please look over your posts before you post them.

When you have your Silver dissolved in Nitric you will get it out with a lot less waste and processing if you just cement it directly on Copper.
After a proper washing you can then melt it and make bars or shots at 99 to 999 pure Silver depending on your skill.
 
That will be the next step.
When he has had a good clean conversion from Silver Chloride.
Probably would have been better to cement on Copper in stead of going via Silver Chloride.

Edit. Added missing word
Maybe there is a video posted on the web so I can understand it better, I would be very grateful.
 
Maybe there is a video posted on the web so I can understand it better, I would be very grateful.
The easiest is to Cement the Silver out.
Dissolve in Nitric as you have done, then take the Silver Nitrate and filter well.
Put your silver Nitrate in a container large enough to have some extra room.
Find a solid piece of Copper and clean it well, if necessary grind it and polish it a bit.
Make a hole in it and hang it in some thread or similar so it is completely submerged in the Silver Nitrate.
Stir it well and then from time to time.
When nothing more happens, lift out the Copper piece and brush the loose material into the vessel.
Take the powder/cement and wash well until the water is clean and have no more color.
What you now have is pure Silver at least 99-999 pure.
Treat it to your own preferences.
If you want it purer, you need to run it through a electrolytic cell.
 