Hi all,

Regarding my adventure in processing tailing for gold and silver I concluded the best way to get the precious metals out would be using cyanide leaching, however there is the bottle roll test to be conducted in lab to find the most optimized solution and balance. Any words on how it can be done at home? Thanks
 
Yes - you can do it in a pail with a mixer. A five gallon pail with a paint mixer would work fine.